Use este identificador para citar ou linkar para este item: https://repositorio.ufpa.br/jspui/handle/2011/8707
Registro completo de metadados
Campo DCValorIdioma
dc.creatorNEVES, Murilo Gaby-
dc.creatorLIMA, Fabrício Viana Pereira-
dc.creatorGURGEL, Júlio de Araújo-
dc.creatorVERCELINO, Célia Regina Maio Pinzan-
dc.creatorREZENDE, Fernanda Soares-
dc.creatorBRANDÃO, Gustavo Antônio Martins-
dc.date.accessioned2017-06-16T12:53:07Z-
dc.date.available2017-06-16T12:53:07Z-
dc.date.issued2016-02-
dc.identifier.citationNEVES, Murilo Gaby et al. Deflection test evaluation of different lots of the same nickel-titanium wire commercial brand. Dental Press Journal Orthodontics, Maringá, v. 21, n. 1, p. 42-46, jan/fev. 2016. Disponível em: <http://www.scielo.br/scielo.php?script=sci_arttext&pid=S2176-94512016000100042&lng=pt&nrm=iso>. Acesso em: 16 jun. 2017. <http://dx.doi.org/10.1590/2177-6709.21.1.042-046.oar>.pt_BR
dc.identifier.issn2177-6709pt_BR
dc.identifier.urihttp://repositorio.ufpa.br/jspui/handle/2011/8707-
dc.description.abstractIntroduction: The aim of this in vitro study was to compare the elastic properties of the load-deflection ratio of orthodontic wires of different lot numbers and the same commercial brand. Methods: A total of 40 nickel-titanium (NiTi) wire segments (Morelli OrtodontiaTM - Sorocaba, SP, Brazil), 0.016-in in diameter were used. Groups were sorted according to lot numbers (lots 1, 2, 3 and 4). 28-mm length segments from the straight portion (ends) of archwires were used. Deflection tests were performed in an EMIC universal testing machine with 5-N load cell at 1 mm/minute speed. Force at deactivation was recorded at 0.5, 1, 2 and 3 mm deflection. Analysis of variance (ANOVA) was used to compare differences between group means. Results: When comparing the force of groups at the same deflection (3, 2 and 1 mm), during deactivation, no statistical differences were found. Conclusion: There are no changes in the elastic properties of different lots of the same commercial brand; thus, the use of different lots of the orthodontic wires used in this research does not compromise the final outcomes of the load-deflection ratio.pt_BR
dc.description.provenanceSubmitted by Luciana Alcantara (lalcantara@ufpa.br) on 2017-06-16T12:52:05Z No. of bitstreams: 2 license_rdf: 0 bytes, checksum: d41d8cd98f00b204e9800998ecf8427e (MD5) Artigo_DeflectionTestEvaluation.pdf: 147430 bytes, checksum: 443552f6acc1c2716d459dac8bab79c5 (MD5)en
dc.description.provenanceApproved for entry into archive by Luciana Alcantara (lalcantara@ufpa.br) on 2017-06-16T12:53:07Z (GMT) No. of bitstreams: 2 license_rdf: 0 bytes, checksum: d41d8cd98f00b204e9800998ecf8427e (MD5) Artigo_DeflectionTestEvaluation.pdf: 147430 bytes, checksum: 443552f6acc1c2716d459dac8bab79c5 (MD5)en
dc.description.provenanceMade available in DSpace on 2017-06-16T12:53:07Z (GMT). No. of bitstreams: 2 license_rdf: 0 bytes, checksum: d41d8cd98f00b204e9800998ecf8427e (MD5) Artigo_DeflectionTestEvaluation.pdf: 147430 bytes, checksum: 443552f6acc1c2716d459dac8bab79c5 (MD5) Previous issue date: 2016-02en
dc.languageporpt_BR
dc.publisherUniversidade Federal do Parápt_BR
dc.relation.ispartofDental Press Journal of Orthodonticspt_BR
dc.rightsAcesso Abertopt_BR
dc.subjectOrtodontiapt_BR
dc.subjectElasticidadept_BR
dc.subjectFios ortodônticospt_BR
dc.titleDeflection test evaluation of different lots of the same nickel-titanium wire commercial brandpt_BR
dc.typeArtigo de Periódicopt_BR
dc.publisher.countryBrasilpt_BR
dc.publisher.initialsUFPApt_BR
dc.citation.volume21pt_BR
dc.citation.issue1pt_BR
dc.citation.spage42pt_BR
dcterms.citation.epage46pt_BR
dc.description.resumoIntrodução: o objetivo deste estudo experimental in vitro foi comparar a as propriedades elásticas da relação carga/deflexão para fios de diferentes lotes de uma mesma marca comercial. Métodos: foram selecionados quarenta segmentos de arcos de níquel-titânio superelástico (NiTi) (Morelli Ortodontia, Sorocaba/SP, Brasil), com diâmetro de 0,016”. Os grupos foram ordenados de acordo com os lotes (lotes 1, 2, 3 e 4). Foram utilizados segmentos com 28mm de comprimento da parte reta (extremidades) dos arcos pré-contornados. Os testes de deflexão foram realizados em uma máquina universal de ensaios EMIC, com célula de carga de 5N e velocidade de 1mm/minuto. A força durante a desativação foi registrada nas deflexões de 0,5; 1; 2 e 3mm. O teste de Análise da Variância (ANOVA) foi utilizado para comparar diferenças entre as médias dos grupos. Resultados: na comparação de força dos lotes em um mesmo ponto de deflexão (3, 2 e 1mm), durante a desativação, não houve diferenças estatísticas. Conclusões: não ocorre alteração nas propriedades elásticas em diferentes lotes da mesma marca. Assim, o uso de diferentes lotes dos fios ortodônticos utilizados nesta pesquisa não comprometeu o resultado final da relação carga/deflexãopt_BR
Aparece nas coleções:Artigos Científicos - FOUFPA/ICS

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
Artigo_DeflectionTestEvaluation.pdf143,97 kBAdobe PDFVisualizar/Abrir


Este item está licenciado sob uma Licença Creative Commons Creative Commons